Need Help With Best Coolant To Use On End Mills

WDG

Registered
Registered
I have been using a water soluble mist and after using my mill a lot recently, I knew it was past time for a good cleaning on the bed. I had to remove the vise, which is a piece of junk, but anyway there was some rust on the table so I had to clean it thoroughly the I took a buffing wheel and polished the table. Before I start to use it again, I would like to know what others think is the best to use. I just have the mist now but have told my wife I wanted a tank with a pump and even showed her one in the Vanguard catalog. The problem is what to use in it. I will have to build splash shields for whatever I do but not too sure I want to use water base coolant. Can anyone give me some guidance on this?
 
Help this guy out please. I moved this thread from the Classifieds.

"Billy G"
 
I pretty much use a very light WD-40 mist for everything except tapping. It is the best I have found for aluminum, and works OK on steel. It won't rust the machine and cleans up easily. Unless you are doing heavy production work, flood coolant is not really needed. I set my mister to dispense about a tablespoon of coolant every 10 minutes of so. At the rate I use my machine, a gallon of WD-40 normally lasts for months.

I do use a water soluble coolant for surface grinding, at about a 10% mix.
 
Get some good quality automotive car wax, clean and was your table. 2 or 3 times is good. The wax should help protect your table. I am using coolmist flood coolant and mix it just a little strong, I don't have any trouble with the table rusting. Some swarf may rust if it's left in the "T" slots.

Mike
 
Most important thing, your concentration is too low if you're getting rusting. I go for price:
http://www.use-enco.com/CGI/INSRIT?PARTPG=INLMKD&PMPXNO=945255&PMAKA=296-2347 is $14 a gallon.

Then go 8 or 10 %. The fogless mister helps you put a bit more on without fogging the room. About a half dozen folks, including myself, have build threads on this. My two cents, this (fogless units) is better than flood. Gives 90% of flood with 10% of the mess.

Karl
 
Get some good quality automotive car wax, clean and was your table. 2 or 3 times is good. The wax should help protect your table. I am using coolmist flood coolant and mix it just a little strong, I don't have any trouble with the table rusting. Some swarf may rust if it's left in the "T" slots.

Mike
Car wax or any paste wax on your table will just ease in the vise slipping during heavy cuts. Although it will stop rust, it might ruin your project.

OP: I'm no coolant expert, but I'd try adding a little more coolant to the water. For aluminum I like Kerosene, but it is messy and the smell sticks around.
 
If I'm not mistaken, WD-40 is flammable?? I do some cutting with a torch and some grinding in my shop and I would hate to get the last three hairs on my head removed. Probably with the amount Jim is talking about that may not be a problem though. I set my air pressure at about 10-15 PSI. Is that too much, just right, too little? It seems kind of hard to tell how the mist is coming out as it's just that a mist. I do have a measuring bottle that is supposed to mix 1 to a gallon and I can certainly increase it to 1.5 PG. I don't have much left so I need to make a decision as to what to purchase next if I don't use the WD-40. The only adjustment I have is the air pressure and the the small valve on the mister head but there is nothing about % or flow. I was at HF a couple of months ago and purchase one of those cheap pumps that go on a garden hose. I thought about using that to flood my surface grinder, and keeping the mister on the mill. I cleaned it real good and put some way oil on it and then put the vise back together after cleaning it and put some white grease on it so I don't think I can do the car wax thing until the next cleaning. Everyone has given me something to think about and I appreciate it very much.
 
Which mister do you have? I have trico mister and run 15psi into it then adjust the air for just enough to clear chips then adjust the coolant just till the temp drops in the air. I get no mist at all.
 
You didn't say what you're cutting and how fast you need to go. Not everyone needs highest-possible speed production flood cooling. When I mill aluminum I have found dry compressed air to work about as well as anything else with far less mess. I use water soluble oil mist if I have to but fortunately i don't have to very often.
 
You didn't say what you're cutting and how fast you need to go. Not everyone needs highest-possible speed production flood cooling. When I mill aluminum I have found dry compressed air to work about as well as anything else with far less mess. I use water soluble oil mist if I have to but fortunately i don't have to very often.[/QUORusting was never a problem until the government dictated that nitrites be removed from coolant concentrates due to the precived threat from nitrosamines; when nitrites were removed, rusting started. I think the nitrites acted to prevent bacterial contamination of the coolants, which seems to deprive them of their rusting resistance, which is now quite short lived, seeming especially when a film of oil covers the coolant and anerobic digestion sets in, and the resultant acidic coolant causes horrible rusting, Having a vise or other similar acessory on the table seems to also create the anerobic condition.
I am no chemist, but this is what I have observed and dealt with; it is a real pain in the ass!
 
Back
Top