We have some Atmos clocks where folks buffed the gold off.
These usually are replated via electroplating, but do not want to send in the clock to get serviced so we can pay too much to get the plating done.
These are brass base metal to likely do not need a primer coat like nickel, but that may allow for a more consistent finish.
We nickel plated a penny 50 years ago, but that was using coins, not too good.
There are plenty of options, different brands, dip type and brush type.
The top frame is maybe 8 by 5 inches so maybe brush type?
Has anyone else went down this road?
The dip type claim to plate in seconds, but how much does one get in a bottle?
Lots to learn, we would rather learn all of the wrong ways...
Sent from my SM-G781V using Tapatalk
These usually are replated via electroplating, but do not want to send in the clock to get serviced so we can pay too much to get the plating done.
These are brass base metal to likely do not need a primer coat like nickel, but that may allow for a more consistent finish.
We nickel plated a penny 50 years ago, but that was using coins, not too good.
There are plenty of options, different brands, dip type and brush type.
The top frame is maybe 8 by 5 inches so maybe brush type?
Has anyone else went down this road?
The dip type claim to plate in seconds, but how much does one get in a bottle?
Lots to learn, we would rather learn all of the wrong ways...
Sent from my SM-G781V using Tapatalk